Esasan jübi telefonynda, senagat kompýuterinde, awtoulag elektronikasynda we OCA çykarylýan filmde ulanylýar.
1. OCA çykarylýan esasy film - GM60 seriýasy , SFP seriýasy
Sypatlar | Bölüm | GM60 / SFP seriýasy | GM60A | GM60B | |||||||
Galyňlyk | μm | 50 | 75 | 100 | 50 | 75 | 100 | 50 | 75 | 100 | |
Dartyş güýji | MD | MPa | 203 | 214 | 180 | 226 | 194 | 210 | 226 | 184 | 210 |
TD | MPa | 239 | 240 | 247 | 251 | 235 | 205 | 251 | 235 | 205 | |
Uzynlygy arakesme | MD | % | 126 | 135 | 151 | 178 | 145 | 152 | 178 | 145 | 152 |
TD | % | 105 | 124 | 121 | 140 | 122 | 136 | 140 | 122 | 136 | |
Gysmak (150 ℃ / 30min) | MD | % | 1.2 | 1.2 | 1.2 | 1.2 | 1.2 | 1.2 | 1.2 | 1.2 | 1.2 |
TD | % | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | |
Geçiriş | % | 90.2 | 90.1 | 90.1 | 90.1 | 90.0 | 89.2 | 90.1 | 90.0 | 89.2 | |
Duman | % | 3.3 | 3.5 | 4.0 | 5.4 | 5.8 | 6.0 | 3.5 | 3.8 | 4.0 |
2. Antistatiki başlangyç film - YM30 seriýasy
Sypatlar | Bölüm | YM30 | YM30A | YM30B | ||||
Galyňlyk | μm | 38 | 50 | 75 | 38 | 50 | 50 | |
Gysmak (150 ℃ / 30min) | MD | % | 1.3 | 1.2 | 1.1 | 1.3 | 1.2 | 1.3 |
TD | % | 0.04 | 0.01 | 0.02 | 0.03 | -0.01 | -0.01 | |
Geçiriş | % | 90.4 | 90.5 | 90.5 | 93.8 | 92.8 | 90.5 | |
Duman | % | 1.89 | 1.94 | 2.35 | 1.97 | 2.4 | 1.94 | |
Faceerüsti garşylyk | Ω | 105-7 | 108-10 | 105-7 | ||||
Faceerüsti reňk | Gök | Reňksiz | Kül gara |
3. Pes oligomer esasy film - GM30 / GM31 / YM40
Sypatlar | Bölüm | GM30 | GM31 | YM40 | ||||
Galyňlyk | μm | 50 | 125 | 50 | 125 | 50 | 125 | |
Gysmak (150 ℃ / 30min) | MD | % | 0.7 | 0.5 | 0.5 | 1.1 | 1.2 | 1.2 |
TD | % | 0.2 | 0.2 | 0.4 | 0.9 | 0.04 | 0.01 | |
Geçiriş | % | 90.2 | 90.3 | 90.2 | 90.1 | 90.2 | 90.3 | |
Duman | % | 1.6 | 1.8 | 2.4 | 3.4 | 2.02 | 2.68 | |
Aýdyňlyk | % | 99.4 | 99.3 | 97.6 | 94.6 | / | / |