Köpugurly epoksi rezin tehniki aýratynlyklary | Gaplamak usuly | Arza | |||||||||||||
Model | Reňk | Forma | Gaty mazmun (%) | EEW (g / eq) | Softumşak nokat (℃) | Hromatika (G / H) | Iscapyşmazlyk (mPa · s) | Gidrolizlenýän hlor (ppm) | Bromyň mazmuny (%) | Fosforyň mazmuny (%) | Mysal | ||||
Köpugurly epoksi rezin | EMTE 350 seriýa | EMTE350 | Gyzyl goňur | Gaty | - | 195-230 | 80-90 | - | 00600 | / | - | Içki PE linerli kagyz halta: 25 kg / halta. | Elektron mis örtükli laminatlar, birleşdirilen materiallar we beýleki meýdanlar. | ||
EMTE350L | 195-230 | 70-80 | 00600 | / | - | ||||||||||
EMTE350LL | 195-230 | 60-70 | 00600 | / | - | ||||||||||
EMTE350H | 195-230 | 90-100 | 00600 | / | - | ||||||||||
Tetrafenol etany Epoksi rezin | EMTE 350A70 | Gyzyl goňur | Suwuk | 70 ± 1.0 | 200-240 | - | G: 12-14 | 50-250 | ≤500 | - | ![]() | Demir deprek: 220kg / deprek |